MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Stoody® 3 Cobalt-Base Cast Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Stood® 3 is a high carbon, chromium, tungsten cobalt-base centrifugally cast alloy designed to be non-magnetic in the as-cast and stress relieved conditions. This alloy exhibits improved wear and corrosion resistance, but has less impact and thermal shock resistance than Stood 1. It is used in applications where a non-magnetic version of Stood is 1 is required and also - as long as some caution is taken towards its slightly low impact strength properties, where additional abrasion resistance is desirable. Stood 3 can be manufactured to conform to Military specification MIL-C-15345F, Alloy 22, and MIL-C-24248 (ships), Composition IV.

Recommended for steel mill guide rolls, bearing bushings, tube forming rolls, rotary seal rings, can and barrel seaming rolls and wear pads.

Information provided by Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Key Words: MIL-C-15345F, Alloy 22, and MIL-C-24248
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 54 - 58
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.2 %
Chromium, Cr 31 %
Cobalt, Co 50 %As remainder
Iron, Fe 1.0 %
Nickel, Ni 1.0 %
Other 1.5 %
Silicon, Si 1.0 %
Tungsten, W 12.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Stoody® 12 Cobalt-Base Cast Alloy
Kennametal Stellite Stoody® 6 Cobalt-Base Cast Alloy
Kennametal Stellite Stoody® 19 Cobalt-Base Cast Alloy
Kennametal Stellite Stoody® 5 Cobalt-Base Cast Alloy
Kennametal Stellite Stellite® STAR cast

NSST3 / 19205

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.