System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Kolon Spelloy® KB132G15VO Polymer Alloy Resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
Material Notes:
Spelloy® is a TPO alloy featuring: High impact resistance (at low temperature), Good dimensional stability, High heat resistance.
Information provided by US distributor, API-Kolon.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.37
g/cc
DIN 53479; ASTM D792
Water Absorption
0.11 %
DIN 53475; ASTM D570
Linear Mold Shrinkage
0.0060
-
0.0080
cm/cm
ASTM D955
Melt Flow
17
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
115
DIN 53505; ASTM D785
Tensile Strength, Ultimate
82.0
MPa
DIN 53455; ASTM D638
Elongation at Break
5.0 %
DIN 53455; ASTM D638
Flexural Yield Strength
147
MPa
DIN 53452; ASTM D790
Flexural Modulus
4.90
GPa
DIN 53452; ASTM D790
Izod Impact, Notched
0.880
J/cm
ASTM D256
Electrical Properties
Original Value
Comments
Dielectric Constant
3.7
@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength
23.0
kV/mm
ASTM D149/DIN 53481
Arc Resistance
110
sec
ASTM D495
Thermal Properties
Original Value
Comments
CTE, linear
40.0
µm/m-°C
@Temperature 20.0 °C
DIN 53752; ASTM D696
Melting Point
220
°C
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi)
160
°C
DIN 53461; ASTM D648
Flammability, UL94
V-0
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLAKO6 / 49849
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.