MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Sulnap® ISO Grade 22 Cutting Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Sulnap Cutting Oil is suited for general-purpose machining operations, such as turning, boring, planing, shaping, light- to medium-duty threading, sawing, hobbing and gear cutting. It can be used for machining ferrous and nonferrous metals, such as carbon and alloy steels, brass, bronze, copper, magnesium and aluminum without the danger of corrosion. Copper-containing metals may discolor slightly. Sulnap Cutting Oil is manufactured with high-viscosity-index paraffinic base oils blended with a chlorine-sulfur additive system. It protects metals from extreme pressures by forming metallic compounds on the face of the chip and tool. It also acts as a lubricant by reducing friction. As the temperature increases during machining, the chlorinated paraffins in the additive system activate. Increasing temperatures and load on the surface activate the sulfur-phosphorus extreme-pressure additive to protect the tip of the tool and the machined surface. The low viscosity of Sulnap Cutting Oil helps dissipate heat rapidly from the cutting surface, producing less discoloration and distortion and providing the necessary cooling for high-speed machining without excessive fogging.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.29 lb/gal
Viscosity Measurement 87Viscosity Index
Saybolt Viscosity at 100°F 104 SUS
Saybolt Viscosity at 210°F 40 SUS
Kinematic Viscosity at 40°C (104°F) 21 cSt
Kinematic Viscosity at 100°C (212°F) 4.1 cSt
ASTM Color 0.50
 
Thermal PropertiesOriginal ValueComments
Pour Point 0.000 °F
Flash Point 395 °F
 
Descriptive Properties
Chlorine1.8 wt. %
Sulfur0.86 wt. %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON154 / 75191

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.