MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® A 2427 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol A 2427 is an aqueous, hydroxyfunctional polyacrylate dispersion. In the formulation of fast-drying, waterborne two-component polyurethane primers and topcoats, as well as one-component coatings.

Properties / Applications: Bayhydrol A 2427 is preferably combined with anionic hydrophilically modified polyisocyanates such as Bayhydur XP 2487/1 to formulate transparent and pigmented primers and topcoats. Topcoats based on Bayhydrol A 2427 and Bayhydur XP 2487/1 are characterized by their good chemical resistance properties, especially their resistance to discoloring liquids. Bayhydrol A 2427 can be used to formulate hard and scratch-resistant one-component coatings for the coating of polystyrene and ABS. The coatings provide high ethanol and creme resistances, especially in one-component metallic monocoat systems. A further advantage of Bayhydrol A 2427 is its good resistance to yellowing. Bayhydrol A 2427 can be combined with polyurethane dispersions in one- and two-component formulations. It can also be combined with UV-curing, waterborne binders. In many cases, this increases the hardness of the formulation, thus improving chemical resistance. Compatibility should be tested in advance in each case. On account of their high reactivity, the formulated two-component coatings have a maximum pot life of 4 hours. The use of two-component spray equipment is therefore recommended, particularly in the case of pigmented formulations. Water, water/acetone mixtures, water/alcohol mixtures (in particular with the addition of 0.5 to 5% N,N-dimethylethanolamine) or alkaline cleaning agents are suitable as cleaning formulation for application equipment. As with any product, use of Bayhydrol A 2427 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Volatiles 56 - 59 %1g/1h/125 °C/convection oven
pH 8.0 - 9.0
Viscosity <= 100 cPD= approx. 40 s-1
 
Descriptive Properties
Content2%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0151 / 201934

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.