MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK NCF 218 Film
Categories: Polymer

Material Notes: Appearance: Transparent yellow film

Product Benefits:

  • Enable fine pitch, narrow gap Cu Pillar
Cure: Heat cure

Application: Semiconductor, Films

Typical Applications: Thermal Compression Bonding

LOCTITE ABLESTIK NCF 218 transparent film is specially formulated for Pb free, low ?, thin gap, large and thin die used in advance flip chip applications. This material is suitable for die to die, die to wafer (TSV) or die to substrate applications.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption 1.20 %
@Temperature 85.0 °C
Saturation, after 85% RH exposure
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 110 MPa
@Temperature 250 °C
Cured, Storage
 6400 MPa
@Temperature 25.0 °C
Cured, Storage
Shear Strength 5.40 MPa
@Temperature 260 °C
Hot Die, 3 x 3 mm SiN die on BT substrate
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°CCured, Below Tg
 190 µm/m-°CCured, Above Tg
Maximum Service Temperature, Air 162 °CDifferential Scanning Calorimetry, On-set temperature
 168 °CDifferential Scanning Calorimetry, Peak temperature
Glass Transition Temp, Tg 119 °Cpost cure TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 minramp to 175ºC, hold 2 hours @ 175°C
Shelf Life 6.00 Month
@Temperature 5.00 °C
Uncured
 
Descriptive Properties
Extractable Ionic Content (ppm)<10Cured, Sodium (Na+)
 <10Cured, Potassium (K+)
 <10Cured, Chloride (Cl-)
Weight Loss (%)1.2TGA @ 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5058 / 255269

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.