Applications Alathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typical customer applications include rigid food packaging such as four, five and six-quart ice cream containers produced at high speeds in fast-cycling, multi-cavity stack molds.Regulatory Status H4262 meets the requirements of the Food and Drug Administration regulation 21 FR 177.1520. Processing Techniques Specific recommendations for processing H4262 can only be made when the processing conditions, equipment and end use are known. |