MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 501/65 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 501/65 is a peroxide crosslinking HCR silicone for the manufacture of silicone-insulated cables and wires.

Properties: Most of the properties of this high performance material today are also found in ELASTOSIL® R 510/70.

Special features:

  • good mechanical and electrical properties
  • good tear strength
  • good heat resistance
  • good rheological properties
  • high extrusion speed
Application: Cable insulations for household, automotive, railway, marine and aerospace applications.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62DIN 53505
Tensile Strength at Break 8.00 MPaDIN 53504 S1
Elongation at Break 460 %DIN 53504 S1
Tear Strength 19.0 kN/mASTM D624 B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmDIN IEC 93
Dielectric Constant 2.9
@Frequency 50 Hz
DIN VDE 0303
Dielectric Strength 24.0 kV/mmDIN IEC 243-1
Dissipation Factor 0.00030
@Frequency 50 Hz
DIN VDE 0303
 
Descriptive Properties
Appearancetranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3071/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3005/60 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R 427/70 High Strength Silicone Base
Wacker Elastosil® R 420/70 Silicone Rubber

PWACK9214 / 204743

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.