MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Pocan® TS 3221 901510 PBT+PET, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PBT, 20% glass fibers, improved toughness, reduced warpage, good surface quality

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183
Filler Content 20 %Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 cm/cmPlaque 60 x 60 x 2mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmPlaque 60 x 60 x 2mm; ISO 294-4
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 270 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 3.3 %Nominal, 50 mm/min; ISO 527-1,-2
Tensile Modulus 5500 MPa1 mm/min; ISO 527-1,-2
Flexural Strain at Yield 3.8 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 40.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 130 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 225 - 250 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °CMethod Af; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °CMethod Bf; ISO 75-1,-2
Shrinkage, MD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
Shrinkage, TD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °CPlaque 60 x 60 x 2mm
Mold Temperature 90.0 °CPlaque 60 x 60 x 2mm
Hold Pressure 60.0 MPaPlaque 60 x 60 x 2mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® S 7926 000000 PBT
Envalior Pocan® C 1202 000000 PBT+PC
DuPont Mobility and Materials Crastin® 6129 NC010 PBT

PLANW9020 / 208476

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.