MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SCG Chemicals EL-Lene™ H511W High Density Polyethylene Wire & Cable Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); HDPE, Fiber Grade

Material Notes: Key Characteristics: Contains special metal deactivator, high mechanical properties, high speed extrusion

Recommended Applications: Insulation of communication cables

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.949 g/ccASTM D1505
ESCR 10% Igepal® >= 168 hour
@Temperature 50.0 °C
F0; ASTM D1693
Oxidative Induction Time (OIT) >= 100 min
@Temperature 200 °C
ASTM D3895
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength at Break 33.0 MPaASTM D638
Tensile Strength, Yield 230 kg(f)/cm²ASTM D638
Elongation at Break >= 600 %ASTM D638
Flexural Modulus >= 8000 kg(f)/cm²ASTM D790
Izod Impact, Notched 14.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.32ASTM D1531
Dielectric Strength 20.0 kV/mmASTM D149
Dissipation Factor 0.000060ASTM D1531
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow HDPE 30460M High Density Polyethylene
Eastman M3006-P Polyethylene
Eastman M30036-P Polyethylene
Dow HDPE 38152M High Density Polyethylene
LyondellBasell Alathon® M5370WC High Density Polyethylene

PSCGC915 / 120669

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.