MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inov Chem Donpipe 311 Water base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonPipe 311 is a kind of blend polyether polyol with water as foaming agent, polyol as the main raw material, mixed with special auxiliary agent. It is developed for propping of water, oil or gas pipelines, furniture and other products,also with moisture proof and heat preservation functions . The polyurethane product prepared by reacting it with isocyanate has the following advantages:
-- Environment friendly, without destroying the ozone layer
-- High compressive strength of foam
-- Fine and smooth Foam cell , with good waterproof and moisture-proof performance

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 - 1.16 g/cc
Density >= 0.100 g/ccMold density; GB/T 6343
 0.0800 - 0.500 g/ccFree density, Manual Mix
 0.0800 - 0.500 g/ccFree density, High Pressure
Viscosity 800 - 1000 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.800 MPaGB/T 8813
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 10.0 °C
GB/T 3399
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CMaterial Temperature, Manual mix
 20.0 - 25.0 °CMaterial Temperature, High pressure
Cure Time 100 - 200 secTack free time, High pressure
 120 - 240 secTack free time, Manual Mix
Gel Time 1.30 - 2.67 minHigh Pressure
 1.67 - 3.30 minManual Mix
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow transparent viscous liquid
Closed-cell rate=90%GB/T 10799
Cream time20-70 secHigh Pressure
 30-80 secManual Mix
Dimensional stability=0.5%24h, -20?; GB/T8811
 =1.0%24h, 100?; GB/T8811
FlammabilityB3, B2, B1GB/T 8624
Hydroxyl value300-400 mgKOH/g
Recommended Ratio100:100-120DonPipe 311/Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM013 / 312542

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.