MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Metallyte™ UHB 35 MWHB OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A multi-layer, cavitaed, white OPP film structure that has exceptional barrier to gases and flavors. It is metalized on one side and treated on the other. It is designed for use in laminations or as a converted monoweb, especially with converter-applied cold seal sealants. The treated face has surface sealing characteristics for fine sealing and will lap seal to some coextruded OPP films.

Availability: Latin America, North America and South America

Key Features:

  • Outstanding opacity
  • Outstanding moisture and oxygen barrier
  • Outstanding aroma and flavor barrier
  • Excellent flex-Crack resistance
  • Excellent surface for high graphic quality
Features:
    Flavor & Aroma Barrier
  • Gas Barrier
  • In Lamination Lap Sealable
  • Light Barrier
  • Moisture Barrier
  • Oxygen Barrier
Applications:
  • Bakery
Uses:
  • HFFS Flexible Packaging
  • Pouches – Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Extrusion Coating, Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Priming, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.0190 g/100 in²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Oxygen Transmission Rate 0.00600 cc/100 in²/dayExxonMobil Method
Thickness 1.40 milExxonMobil Method
Coating Weight 15.5 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Break, MD 10900 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 12300 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 5.0 %
@Temperature 135 °C
ExxonMobil Method
 
Descriptive Properties
Treatment40 dyne/cmTreated Surface
Yield27900 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Metallyte™ 15MM288 OPP Film
ExxonMobil Metallyte™ UHB 35MU842 OPP Film
ExxonMobil Metallyte™ 18MM383 OPP Film

PEX99529 / 175765

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.