MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLTHANE® D16N90UV Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® D16N90UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of transparent, colorless pellets, offering adequate hardness, excellent mechanical properties and good hydrolysis and microbial resistance. PEARLTHANE® D16N90UV is designed for extrusion and injection processes.

PEARLTHANE® D16N90UV is especially designed for extrusion of tubes and profiles and injection molding of technical parts where excellent mechanical properties at low temperature, hydrolysis and microbe resistance are required.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Tensile Strength, Yield 6530 psiASTM D412
Elongation at Break 450 %ASTM D412
100% Modulus 1.16 ksi
@Strain 100 %
ASTM D412
300% Modulus 2.901 ksi
@Strain 300 %
ASTM D412
Tear Strength 742 pliASTM D624 (Die C)
Abrasion 40loss (mm³); DIN 53.516
 
Thermal PropertiesOriginal ValueComments
Melting Point 338 - 356 °FMQSA 111
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Feed Temperature 383 °F
Nozzle Temperature 401 °F
Zone 1 410 °F
Zone 2 419 - 437 °F
Zone 3 446 - 464 °F
Zone 4 392 - 410 °F
Die Temperature 392 - 410 °F
Mold Temperature 95.0 °F
Moisture Content <= 0.10 %MQSA 44
Screw Speed 50 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMES61b / 109239

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.