MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi TOUGH PLA 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: TOUGH PLA is engineered for its high impact and strength like ABS and the stiffness of PLA. The material shows excellent results in layer adhesion and is the perfect match for tooling or manufacturing aids where a high impact is needed. TOUGH PLA is a plug & play material and printable on a wide range of temperatures.

Features:

  • High impact and stiffness
  • Prints like regular PLA (easy to print)
  • No warpage & no shrinkage
  • Printable with various print temperatures
  • Suitable for applications which needs to be strong
  • Industrial touch and feel
Colors: RPLA is available from stock in Black.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccISO 1183
Filament Diameter 1750 µmTolerance: 50 µm, =95% Roundness
 2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 8.75 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 19.0 MPaISO 527
Tensile Strength, Yield 46.0 MPaISO 527
Elongation at Break 27 %ISO 527
Elongation at Yield 2.0 %ISO 527
Tensile Modulus 2750 MPa(E); ISO 527
Charpy Impact, Notched 29.8 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 57.0 °CISO 306 B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 220 °CPrinting Temperature
 
Descriptive Properties
Bed Temp=60°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9850 / 301075

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.