MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Verdant Specialty Solutions GLOKILL® PQ60 Surfactant
Categories: Fluid

Material Notes: Description: Algicide and biocide for swimming pool

Identification: POLYQUARTERNARY AMMONIUM CHLORIDE, AQUEOUS SOLUTION

CAS: 25988 – 97 – 0

Available in: Europe

Function: Algaecide for use in Industrial Water Treatment and Swimming Pool applications

Stability: Stable in hard water. Stable in normal use dilutions in the presence of up 40 ppm chlorine. Stable in acidic, neutral and mildly alkaline solutions.

Compatibility: Compatible with most types of non-ionic, cationic, betaines and ampholytes. Incompatible with anionics.

Applications: Glokill PQ 60 is a non foaming and non-wetting biocide for use as algaecide in swimming polls & cooling water applications. It is a long lasting, non-volatile product that does not smell and is not corrosive to water systems. In swimming pool applications Glokill PQ 60 is compatible with commonly used bactericides and is effective against most forms of algae. Rhodia is supporting the active ingredient in Glokill PQ 60 towards Annex 1 listing under the BDP (98/8/EC) as an algaecide for Product Type 2 : Private area and public health area disinfectants and other biocidal products and Product Type 11 : Preservatives for liquid cooling & processing systems.

Information provided by Rhodia, Rhodia has been acquired by Solvay. Verdant Specialty Solutions was created through the purchase of Solvay's amphoteric and secondary surfactants business

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 - 1.19 g/cc
pH 5.7 - 6.25% aq. Sol; L100
Viscosity 4.0 - 8.0 cP20% aq. Sol.; L170
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceColorless to pale yellow
Assay59-61%L010
CompositionFree Amine<0.2%, L260
Ionic ChargeCationic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD140 / 137371

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.