MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ryton® R-7-232NA PPS, Glass/mineral filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Glass/mineral filled, high temperature and hydrolysis resistance, FDA & EU-Food approved

Ryton® R-7-232NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature environments.

Ryton R-7-232NA complies with United States Food and Drug Administration (FDA) and European Union food contact regulations.

Applications: Food Service Applications

Features: Good Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.97 g/ccASTM D792
Water Absorption 0.013 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0018 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0057 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 101ASTM D785
Hardness, Rockwell R 121ASTM D785
Tensile Stress 150 MPaISO 527-2
Elongation at Break 1.0 %ISO 527-2
Tensile Modulus 21500 MPaISO 527-2
Flexural Strength 230 MPaISO 178
Flexural Modulus 20500 MPaISO 178
Compressive Strength 265 MPaASTM D695
Poissons Ratio 0.34ASTM E132
Izod Impact, Notched 66.0 J/m
@Thickness 3.18 mm
ASTM D256
Izod Impact, Unnotched 300 J/m
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 20.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+16 ohm-cmASTM D257
Surface Resistance 5.20e+15 ohmASTM D257
Dielectric Constant 4.13
@Frequency 1000 Hz
ASTM D150
 4.16
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.0 kV/mmASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 0.0040
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 190 secASTM D495
Comparative Tracking Index 225 VUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 11.0 µm/m-°C
@Temperature 120 - 200 °C
ASTM E831
 12.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
 13.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 26.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
 37.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
 79.0 µm/m-°C
@Temperature 125 - 200 °C
ASTM E831
Thermal Conductivity 0.310 W/m-KASTM C177
Melting Point 285 °C
Maximum Service Temperature, Air 220 - 240 °CUL Temperature Rating
Deflection Temperature at 1.8 MPa (264 psi) 262 °CUnannealed; ASTM D648
Flammability, UL94 V-0
 5VA
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4452 / 280252

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.