T-BLEND® is a series of thermoplastic rubber compound materials produced by TSRC Corporation. T-BLEND® 1903-45N can be applied to a variety of unique products with the advantages of rebound resilience, compression and bending properties by injection molding. T-BLEND® 1903-45N is a palletized elastomer compound based on Styrenic Block copolymer. It’s produced in pellet to manufacture conveniently. T-BLEND® 1903-45N thermoplastic elastomer compound is recyclable including wastes from gate, runner, and waste parts.Information provided by TSRC Corporation |