MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene PP1510PC Polyolefin, Wire/Cable Grade
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: Petrothene PP1510PC is selected for use as primary insulation or a jacketing base resin for wire and cable applications. PP1510PC contains antioxidants to help ensure thermal stability during processing and to provide excellent long-term aging properties. It also contains a metal deactivator to prevent degradation while the cable is in service. Petrothene PP1510PC meets the requirements of the following: ASTM D 4101, Group 03, Class 4, Grade 8; PP0348B44803EO; Federal LP394C, Type IV, Grade B. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D1505
ESCR 100% Igepal® >= 168 hour0 failures @ 7 days, cond. A
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 28.6 MPaASTM D638
Tensile Strength, Yield 22.1 MPaASTM D638
Elongation at Break 600 %ASTM D638
Flexural Modulus, 1% Secant 1070 MPaASTM D790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 2.27
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -25.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Feed Temperature 224 - 241 °C
Zone 2 221 - 238 °C
Zone 3 200 - 210 °C
Zone 4-x 185 - 196 °C
Adapter Temperature 204 - 218 °C
Die Temperature 216 - 238 °C
 
Descriptive Properties
Processing MethodWire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom PP HH42L 356015 Polypropylene
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene Copolymer

PEQT8872 / 220506

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.