MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of atmospheres. Available as wire and strip. Slightly magnetic.

Information provided by Resistalloy International Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 180
Tensile Strength, Ultimate 750 MPa
 100 MPa
@Temperature 900 °C
Tensile Strength, Yield 450 MPa
Elongation at Break 25 - 30 %
@Thickness 50.0 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 668 ohm-cir-mil/ftTemperature Factor is 1.10 at 800°C (1470°F). Temperature Factor is 1.11 at 1000°C (1830°F). Temperature Factor is 1.13 at 1200°C (2190°F).
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 250 °C
 15.0 µm/m-°C
@Temperature 20.0 - 500 °C
 17.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 13.0 W/m-K
Melting Point 1390 °C
Maximum Service Temperature, Air 1150 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.88Fully Oxidized
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 15 %
Iron, Fe 25 %
Nickel, Ni 60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel
Resistalloy International Fecralloy™ Electrical Resistance Steel

NRESIST1 / 18828

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.