MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Petromont 2100 Medium Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Petromont HDPE 2100 is a medium density polyethylene blown film resin produced using the UNIPOL™ Process. This resin is designed specifically for blown film made by co-extrusion. It is commonly used in HDPE resins in applications where an improvement in the film resilience property is required, and with LLDPE where higher stiffness is required.

Petromont HDPE 2100 has a broad molecular weight distribution. This, combined with its medium molecular weight and medium density, results in excellent processing characteristics at high extrusion rates with good flexibility and resilience. The excellent draw down characteristics permit production of high quality thin films

Key Words: Film
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D1505
Melt Flow 0.20 g/10 minI2; ASTM D1238
 20 g/10 minI21; ASTM D238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 32.0 MPaASTM D638
Elongation at Break >= 800 %ASTM D638
Flexural Modulus 0.690 GPaat 1% elongation; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °CPetromont
Vicat Softening Point 116 °CASTM D1525
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin
Borealis Borstar® FB1350 Medium Density Polyethylene
Bayport Polymers Baystar™ Lumicene® mPE M 3410 EP MDPE Film, sheet
Chevron Phillips Marlex® HHM TR-130 MDPE Film Resin

PPETROM08 / 56202

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.