MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper-Nickel, Chromium Bearing, UNS C72200, H04 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Soldering, Brazing, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding

Common Fabrication Processes: Bending; Forming; Welding

Typical uses: Condenser Tubing; Heat Exchanger Tubing; Salt Water Piping

Applicable Specifications: Bar – ASTM B122/B122M; Condenser & Heat Exchanger Tube with Integral Fins – ASTM B956/B956M; Pipe – ASTM B466/B466M; Pipe – ASTM B466/B466M; Plate - Condenser Tube ASTM B171/B171M, ASTM B122/B122M; Sheet – ASTM B122/B122M; Strip – ASTM B122/B122M; Tube – ASTM B543/B543M, Condenser Tube ASTM B111/B111M; ASTM B395/B395M, ASTM B552, ASTM B359/B359M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.0 ksi
Tensile Strength, Yield 66.0 ksi0.2% Offset
Elongation at Break 6.0 %
Tensile Modulus 20000 ksi
Modulus of Rigidity 8200 ksi
Poissons Ratio 0.22Calculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000260 ohm-cm6.53% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0940 BTU/lb-°F
Thermal Conductivity 19.9 BTU-in/hr-ft²-°F
Melting Point 2052 - 2148 °F
Solidus 2052 °F
Liquidus 2148 °F
Annealing Point 1350 - 1500 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1650 - 1900 °F
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 0.30 - 0.70 %
Copper, Cu 78.2 - 84.2 %As Balance
Iron, Fe 0.50 - 1.0 %
Lead, Pb <= 0.050 %
Manganese, Mn <= 1.0 %
Nickel, Ni 15 - 18 %
Silicon, Si <= 0.030 %
Titanium, Ti <= 0.030 %
Zinc, Zn <= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC72200x2 / 293096

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.