Excellent properties:- abrasive stability
- high stiffness (E-modulus)
- resistance even at high temperatures
- good grindability
PEAK DISPAL materials allow the manufacturing of pistons for highest operational demands. Property data for Heat Treatment Condition T4 (Quenching in water at RT). Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH. |