MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Struktol POLYDIS 3615 Elastomer modified epoxy prepolymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Epoxy

Material Notes:

Applications: STRUKTOL VP 3615 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural and peel strength. Contrary to PD 3614 the Tg decrease less, but fracture toughness is on the same level.

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/cc
Viscosity 250000 cP
@Temperature 25.0 °C
Dynamic
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Monthin original sealed containers at temperatures less than 40°C
 
Descriptive Properties
AppearanceYellowish, high viscous epoxy resin
Elastomer Content %40 NBR
Epoxy Equivalent Weight (g/Eq)300
Resin-base of the prepolymerDGEBA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Struktol POLYDIS 3610 Reactive, elastomer modified epoxy prepolymer (block-copolymer)
Struktol VP 3695 Elastomer modified epoxy prepolymer
Struktol VP 3643 Optimized elastomer-modified epoxy prepolymer
Struktol POLYDIS 3691 Elastomer modified epoxy prepolymer
Struktol POLYDIS 3622 Elastomer modified epoxy prepolymer

PSTRUK56 / 69283

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.