Hostacom TRC 483N G82718 is a 17% talc filled PP copolymer, with good flowability, good stiffness, excellent impact resistance and very good scratch resistance. The product is also available as a customized color matched, pellet form. This grade is delivered in G82718 color version. Applications: Instrument PanelsInformation provided by LyondellBasell. |