MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Redwood Plastics Redco™ FRP GRATING
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.72 - 1.94 g/ccASTM D792
Water Absorption 0.45 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 45ASTM D2583
Tensile Strength 7000 psiCW; ASTM D638
 30000 psiLW; ASTM D638
Modulus of Elasticity 2800 ksi
Tensile Modulus 800000 psiCW; ASTM D638
 2.50e+6 psiLW; ASTM D638
Flexural Strength 10000 psiCW; ASTM D790
 30000 psiLW; ASTM D790
Flexural Modulus 800000 psiCW; ASTM D790
 1.80e+6 psiLW; ASTM D790
Compressive Strength 15000 psiCW; ASTM D695
 30000 psiLW; ASTM D695
Compressive Modulus 100000 psiCW; ASTM D695
 2.50e+6 psiLW; ASTM D695
Shear Modulus 3.10 GPa
Shear Strength 4500 psiShort Beam; ASTM D-2344
 10000 psiPunch; ASTM D-732
Izod Impact, Notched 216 J/mCW; ASTM D256
 1350 J/mLW; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 200 V/milASTM D149
Arc Resistance 120 secLW; ASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°CASTM D696

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW122 / 296688

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.