Injection molding grade; with high mechanical strength for articles subject to wear; excellent abrasion resistance; good wear resistance; very easy release; very short cycle times; opaque to translucent; Cylindrical pellets; Rollers; Ear-tags; Technical parts Mechanical property data for samples at 50% RH. Information provided by Covestro |