High fluidity grade for optical media that provides low optical distortion moldings. Impurities in pellets are severely controlled, and resulting high quality is obtaining good reputation. Applications: Optical disc moldings such as CD, CD-ROM, MO, MD and DVD.Optical lens moldings.Information provided by Teijin Chemicals Ltd. |