MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bakelite® PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Phenolic molding compound, mainly organically filled, very soft flow for large molds.

Applications: Housing parts, heat shields, cookware fittings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Apparent Bulk Density 0.620 g/ccISO 60
Linear Mold Shrinkage 0.0070 cm/cmCompression Molding. Post Shrinkage = 0.55%.; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 280 MPaH961/30; ISO 2039/P1
Tensile Strength 60.0 MPaISO 527 - 1/2
Tensile Modulus 7500 MPaISO 527 - 1/2
Flexural Strength 90.0 MPaISO 178
Flexural Modulus 7000 MPaISO 178
Compressive Strength 240 MPaISO 604
Charpy Impact Unnotched 6.00 kJ/m²ISO 179-1 eU
Charpy Impact, Notched 1.30 kJ/m²ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm
Surface Resistance 1.00e+10 ohm
Dielectric Constant 15.5
@Frequency 100 Hz
Dielectric Strength 15.5 kV/mm
@Thickness 1.00 mm
IEC 60243-P1
Dissipation Factor 0.30
@Frequency 100 Hz
Comparative Tracking Index 125 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 8.0 MPa 100 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 75.0 °CInjection molding
Nozzle Temperature 80.0 - 100 °CInjection molding
Melt Temperature 80.0 - 100 °CInjection molding
Mold Temperature 160 - 190 °CInjection molding
 160 - 190 °CCompression molding
Injection Pressure >= 15.0 MPaCompression and injection cavity mold pressure
Back Pressure 0.500 - 2.00 MPaInjection molding
Cure Time 10.0 - 20.0 secPer 1 mm of wall thickness, injection molding
 20.0 - 40.0 secPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Chromatic SpectrumSubdued Colors
Creep Rupture StrengthGood
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceGood
Thermal ExpansionSlight
Water absorption (mg)8024h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Bakelite® PF 1110 Phenolic Molding Compound
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage

PBAKE039 / 27073

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.