A quality, low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips, flexible gaskets and extruded shapes. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |