MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Cavamax® W7 PHARAM BETADEX Beta-cyclodextrin
Categories: Other Engineering Material

Material Notes: CAVAMAX® W7 is pharmaceutical grade betacyclodextrin. CAVAMAX® W7 with seven glucose units has the midsize cavity of the parent cyclodextrins. It is useful for stabilizing, solubilizing or delivering intermediate size molecules, e.g. menthol.

Empirical formula: C42H70O35

CAS No.: 7585-39-9

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 - 0.700 g/cc
pH 5.0 - 8.01% aqueous solution
Molecular Weight 1135 g/mol
Ash <= 0.1 %Residue on ignition
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %1% aqueous solution; 'Clear' but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 14 %
 
Descriptive Properties
Appearanceclear1% aqueous solution
 solid -powder
Colorwhite
Content<0.05Light absorbing impurities of a 1% aqueous solution (350-750 nm)
 <0.1Light absorbing impurities of a 1% aqueous solution (230-350 nm)
 <0.2%Reducing substance (determined as dextrose)
 <0.25%Related substance (alpha-Cyclodextrin)
 <0.25%Related substance (gamma-Cyclodextrin)
 <100/gMolds and yeasts
 <1000/gMicroorganisms
 <5 ppmHeavy metals
 <5 ppmVolatile organics
 0 in 10 gSalmonella/E Coli
 98-101%Content (on dry basis)
Content (%)0.5Related substances (other sugar)
Solubility18.5 g/lOECD 105, in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9052 / 204581

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.