Composition: This system is consist of four components, polyol, ISO, curing agent and catalyst. Characteristics: Mixing Temperature 30~40?, Curing Temperature 80~90?, Demould time 8~10 min (adjustable), the Hardness of finished product could be adjusted by changing the materials ratio of component A+C/B. Mass ratio: DX3520-B: 68 DX3580-A: 96 DX3580-C: 4 Catalyst / DX3580-A: 0.27% Defoaming agent / DX3580-A: 0.47% Information provided by Shandong INOV Polyurethane Co., Ltd. |