MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ G-508 Engineered Specialty Foam
Categories: Other Engineering Material

Material Notes: JFoam™ G-508 is used for structural panels, insulation, and potting applications.

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/ft³
Water Absorption 0.030 %
@Time 86400 sec
10' head
Viscosity 310 cP
@Temperature 48.9 °C
T Component
 435 cP
@Temperature 43.3 °C
T Component
 620 cP
@Temperature 37.8 °C
T Component
 870 cP
@Temperature 32.2 °C
T Component
 1325 cP
@Temperature 26.7 °C
T Component
 1750 cP
@Temperature 21.1 °C
T Component
 3250 cP
@Temperature 48.9 °C
R Component
 4500 cP
@Temperature 43.3 °C
R Component
 9000 cP
@Temperature 37.8 °C
R Component
 16250 cP
@Temperature 32.2 °C
R Component
 23500 cP
@Temperature 26.7 °C
R Component
 28750 cP
@Temperature 21.1 °C
R Component
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 150 psiPerpendicular, 10% deflection; ASTM D1621
 180 psiParallel, 10% deflection; ASTM D1621
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.260 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 180 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Closed Cell Content95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSIX029 / 190956

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.