MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Spruce Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Key Words: Pinus Glabra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.410 g/ccGreen, based on volume
 0.440 g/cc12% moisture content, based on volume
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2002 NGreen
 3292 N12% moisture content
Modulus of Elasticity 1000 ksiGreen
 1230 ksi12% moisture content
Modulus of Rupture 6.00 ksiGreen
 10.4 ksi12% moisture content
Compressive Strength 280 psiGreen, perpendicular to grain
 730 psi12% moisture content, perpendicular to grain
 2840 psiGreen, parallel to grain
 5650 psi12% moisture content, parallel to grain
Shear Strength 900 psiGreen, parallel to grain
 1490 psi12% moisture content, parallel to grain

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Northern White Pine Wood
Southern Pine Wood
American Pine Wood
Western White Pine
Lodgepole Pine Wood

PTSU011 / 71453

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.