MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ RTA3263EUV/1 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ RTA3263EUV/1 fractional melt flow, 1,700 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness, impact strength, weather resistance and processability. It was designed primarily for extruded automotive exterior profile applications. Uses: Automotive exterior parts, profiles

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ISO 868
Tensile Strength, Yield 3340 psiISO 527-1, -2
Elongation at Break 500 %ASTM D638
Flexural Modulus 203 ksiTangent, 0.05 in/min; ASTM D790
 247 ksiTangent, 0.5 in/min; ASTM D790
Gardner Impact 212 in-lb
@Temperature -30.0 °C
ASTM D3029
Dart Drop, Total Energy 24.0 J
@Temperature -30.0 °C
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
Tear Strength 910 pliASTM D624
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 147 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 111 °FUnannealed; ISO 75A-1, -2
Shrinkage 0.90 %Tool, 100x150x3.2 mm; Basell Test Method
 1.1 %
@Temperature 121 °C,
Time 3600 sec
Afterbake, 100x150x3.2 mm; Basell Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer

PMO803 / 53792

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.