Product: PLEXIGLAS® Film WF003 is a high weather resistant, glossy, and white acrylic film for graphic printings and high quality laminations. Due to its excellent performance under long term weathering and UV light exposure, PLEXIGLAS® Film WF003 does not present color change or yellowing. Its glossy and very smooth surface leads the film to have an excellent printing quality. Application: PLEXIGLAS® Film WF003 can be used to be printed on as high quality film decoration and then laminated on different polymeric films and sheets. Laminated decoration films protected by PLEXIGLAS® are suitable for a wide range of molding processes such as thermoforming, and insert molding. PLEXIGLAS® Film WF003 can be used as a single face layer in high UV and weathering resistant durable labels and tapes without the need for an overlay film. The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm). |