MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Redwood Plastics REDCO™ MD Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Redco™ Nylon MD is a moly-filled (molybdenum disulphide filled) grade resulting in superior wear-resistance allowing for longer part life and decreased mating component wear, resulting in less down time.

Typical Applications: Sheaves used in the mobile crane industry, bushings, wear pads for telescoping booms, as well as gears and rollers found in numerous material handling systems, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
Water Absorption 1.25 - 5.0 %Equilibrium
 0.60 - 1.2 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 10500 - 12000 psi
@Time 86400 sec
Elongation at Break 20 - 40 %
Tensile Modulus 350000 - 460000 psi
Flexural Strength 12500 - 17000 psi
Flexural Modulus 350000 - 450000 psi
Compressive Strength 15000 psi10% Deflection
Coefficient of Friction 0.36 - 0.42Dry vs.Steel
Limiting Pressure Velocity 3000 psi-ft/min
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW033 / 296599

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.