MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 216C03 Flexible Plastic Bonder
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 216C03 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermoplastic substrate. TRA-BOND 21C03 is low viscosity and easy to apply. It has an easy 1:1 mix ratio and can be cured at room temperature. This high technology system was formulated for applications in the automotive, medical, aerospace, photonic and assembly industries and can be used anywhere that requires excellent chemical fastening to plastic parts.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccCured
Viscosity 16000 cP16000 cPMixed (lv #4, 12 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90901 hr @ 65°C
 909024 hrs @ 25°C
Adhesive Bond Strength 7.24 MPa1050 psiLap shear, alum to alum, 24 hrs @ 25°C
 10.3 MPa1500 psiLap shear, alum to alum, 1 hr @ 65°C
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 18.0 °C64.4 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
 
Descriptive Properties
Color AmberCured
Mix Ratio, parts by weight1/1Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC043 / 70971

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.