QUINN XT soft tone is an extruded acrylic sheet with the appearance and feel of traditional frosted glass but without the limitations of size and weight. QUINN XT soft tone offers a wide range of creative possibilities for building and industrial glazing, decoration, lighting and advertising, … thanks to its outstanding properties: - Improved light scatter
- Stylish
- trendy look
- Avoids reflective effects
- Easy to maintain, handle, fabricate and form
- High light transmission
- Good optical properties
- Over lengths available
- Stable thickness tolerances
- Interior decoration
- Information signs
- Displays
- Showcases
- Shop fittings
- Advertising signs
- Advertising media
Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |