MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT CHT-BeauSil™ AMO 8928 EM Silicone polymer
Categories: Other Engineering Material

Material Notes: Description: This product is a personal care nonionic microemulsion of aminefunctional silicone polymer.

Key Features

  • Superior conditioning agent
  • Improves wet combing and dry feel
  • Forms substantive, soft films on many different substrates
  • Compatible with cationic, anionic, and nonionic surfactants
Key Applications
  • Shampoo
  • Conditioner
  • Leave-on styling products
  • Lotions and sunscreens
Application: CHT-BeauSil™ AMO 8928 EM is a 28% actives microemulsion of an amine-functional silicone polymer using nonionic surfactants. This nearly transparent microemulsion has industry leading performance, stability, and clarity due to a small and consistent particle size.

INCI Name: Propoxytetramethyl Piperidinyl Dimethicone (and) Trideceth-6 (and) C11-15 Alketh 7

INCI Name Formerly: Propoxytetramethyl Piperidinyl Dimethicone (and) Trideceth-6 (and) C11-15 Pareth 7

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 72 %
pH 5.0
Storage Temperature 4.00 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceColorless microemulsion to opalescent
IonicityNon-ionic
MIT FreeNo
Ultralow cyclic contentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL265 / 314748

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.