MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin RN0612 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimensional stability and high flow, this resin also uses non-chlorinated, non-brominated FR additives with a specific density of 1.1 g/cm^3. NORYL RN0612 may be an excellent material candidate for flat panel TV enclosure applications requiring good rheological properties, heat resistance, hydrolysis resistance and low density.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Viscosity 13 cP
@Load 1.20 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 34 cP
@Load 2.16 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 42.0 MPa50 mm/min; ISO 527
 43.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 42.0 MPa50 mm/min; ISO 527
 43.0 MPa50 mm/min; ASTM D638
Elongation at Break 15 %50 mm/min; ASTM D638
 17 %50 mm/min; ISO 527
Elongation at Yield 1.0 %50 mm/min; ASTM D638
 1.0 %50 mm/min; ISO 527
Tensile Modulus 2100 MPa50 mm/min; ASTM D638
 2100 MPa1 mm/min; ISO 527
Flexural Strength 60.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 64.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2100 MPa1.3 mm/min, 50 mm span; ASTM D790
 2100 MPa2 mm/min; ISO 178
Izod Impact Notched 52.0 JASTM D256
 41.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 4.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 3.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cmASTM D257
 3.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmASTM D257
 1.00e+16 ohmROA; IEC 60093
Dielectric Constant 2.76
@Frequency 1e+6 Hz
ASTM D150
 2.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0035
@Frequency 1e+6 Hz
ASTM D150
 0.0035
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 VIEC 60112
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 96.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 96.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 78.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 95.0 °CRate B/50; ASTM D1525
 95.0 °CRate B/50; ISO 306
 98.0 °CRate B/120; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
UL 94
 V-0
@Thickness >=3.00 mm
UL 94
Glow Wire Ignition Temperature 725 °C
@Thickness 1.00 mm
IEC 60695-2-13
 725 °C
@Thickness 2.00 mm
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 280 °C
Zone 2 240 - 270 °C
Zone 3 260 - 295 °C
Melt Temperature 260 - 295 °CInjection Molding
Mold Temperature 45.0 - 70.0 °C
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 65.0 - 85.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82464 / 290411

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.