MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borcycle™ ME7153SY Polypropylene, 50% Post-consumer Recycled polymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Borcycle" ME7153SY is a natural, UV stabilized, colorable, medium density (MD) jacketing compound. It contains 50% post consumer recyclate (PCR) and is intended for use in medium and low voltage cables.

Typical characteristics:

  • Consistent product properties
  • Low odor
  • Superior processability
  • Low water permeability
  • Excellent environmental stress cracking resistance (ESCR)
  • Easy to color
  • Smooth surface finish
  • Carbon footprint savings
Applications: Borcycle" ME7153SY is intended for following applications: Jackets for energy and communication cables

Specifications: Borcycle" ME7153SY is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures.

  • ASTM D1248 Type II, Class A, Category 4, Grade E8, E9, J4
  • HD 603 S1 DMP 6
  • DIN VDE 0818
  • IEC 60502 Part 2, Type ST7
  • EN 50290-2-24
  • IEC 60840 Type ST7

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.938 g/ccISO 1183-1
ESCR 10% Igepal® >= 2000 hour
@Temperature 50.0 °C
IEC 60811-406
Oxidative Induction Time (OIT) 40.0 min
@Temperature 200 °C
ISO 11357-6
Melt Flow 0.700 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 2.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58.0
@Time 1.00 sec
ISO 868
Flexural Modulus 650 MPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10.0 ohm-cmDC; IEC 60093
Dielectric Strength 20.0 kV/mmIEC 60243
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 210 °C
Drying Temperature <= 70.0 °CPre-heating
Shelf Life 24.0 Month
 
Descriptive Properties
Pressure Test at High Temperature (%)11115 °C, 6h; IEC 60811-508

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9637 / 322994

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.