MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beologic Beobase 05 PE cotton RTM029 Black Rotomolding
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Main properties: jeans look. Applications: indoor products, household, gardening

Information provided by Beologic.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183-1
Melt Flow 4.0 - 4.5 g/10 min
@Load 2.16 kg,
Temperature 90.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13.1 MPaISO 527-1
Tensile Strength 16.1 MPaISO 527-1
Elongation at Break 500 %ISO 527-1
Tensile Modulus 470 MPaISO 527-1
Flexural Modulus 520 MPaISO 178
Charpy Impact, Notched 12.5 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 67.4 °CB120; ISO 306
 
Descriptive Properties
Beologic Article Number595020029
Carbon footprint (kg CO2 eq/kg)2.027PAS 2050
Dry flow rate22-25 sec
Natural fiber content (%)5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBEOL9803 / 314089

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.