MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Manganese Bronze A, UNS C67500, O60 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Soft Anneal

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Hot Forging and Pressing; hot heading and upsetting

Typical uses: Clutch Disks; Pump Rods; Shafting; Bolts; Aircraft Parts; Balls; Bushings; Valve Bodies; Hardware

Applicable Specifications: Bar – ASTM B124/B124M, SAE J463, ASTM B138/B138M SAE J461; Bolts – ASTM F468; Die – Forgings SAE J461, Forgings SAE J463; Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Nuts – ASTM F467; Rod – Forgings ASTM B124/B124M, SAE J461, ASTM B138/B138M, SAE J463; Screws – ASTM F468; Shapes – SAE J463, ASTM B124/B124M, SAE J461, ASTM B138/B138M; Studs - ASTMF468

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.302 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 65
@Thickness 25.4 mm
Tensile Strength 65.0 ksi
@Thickness 25.4 mm
Tensile Strength, Yield 30.0 ksi
@Thickness 25.4 mm
0.5% Ext
Elongation at Break 33 %
@Thickness 25.4 mm
Tensile Modulus 15000 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.34Calculated
Machinability 30 %
Forgeability 80 %
Shear Strength 42.0 ksi
@Thickness 25.4 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000210 ohm-cm8.36% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.8 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 61.0 BTU-in/hr-ft²-°F
Melting Point 1590 - 1630 °F
Solidus 1590 °F
Liquidus 1630 °F
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1150 - 1450 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.25 %
Copper, Cu 57 - 60 %
Iron, Fe 0.80 - 2.0 %
Lead, Pb <= 0.20 %
Manganese, Mn 0.050 - 0.50 %
Tin, Sn 0.50 - 1.5 %
Zinc, Zn 37.4 - 41.7 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialNo

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC67500x3 / 293084

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.