Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample. Data Provided by the manufacturer, Coors Ceramics Co. |
Coors Mullite, 3Al2O3.2SiO2, S2 |