The temperature control setting is 4 and the flash point is 514°F (267°C). The auto ignition is 807°F (431°C). The ball and ring soft point is 190°F (88°C); ASTM E-28-6-7. The peal strength on canvas is 14 PIW at 72°F (22°C). The bonding range of a 1/8 inch bead on Douglas Fir to Douglas Fir is 40 seconds. The delivery rate is 55 seconds for 1 inch x 3 inch cartridge. The ingredients of the product when dried after application are listed as indirect food additives under FDA regulation 21 CFR 175.105. Can bond many plastics, polyolefins. Good impact resistance at low temperature. Information provided by 3M Adhesives Division. |