Softell TKS 209N NAT is an unfilled PP copolymer, with very low rigidity, good scratch resistance and very low gloss. Product is also available as a customized color matched, pellet form. This grade is delivered in natural color version. Applications: Automotive Parts, Interior TrimsInformation provided by LyondellBasell. |