MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Meyors Chemical Rubber Accelerator MBTS(DM) Powder
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD-AC002-00 PT
Chemical Name: 2,2’-dibenzothiazyl disulfide
Trade Name: Rubber Accelerator MBT (M)
CAS No.: 120-78-5
Molecular Formula: C14H8N2S4

Typical Properties: Light yellow powder, The relative density is 1.45~1.50. In room temperature, it slightly dissolved in benzene, toluene, carbon tetrachloride, trichlorobenzenes, acetone, ethanol, ethyl ether, and not dissolve in water, ethyl acetate, petrol and lye.

Recommended Applications: It gives moderate processing safety and moderately fast cures with flat plateau. The vulcanizate characteristics are similar to those obtained with MBT. In fact, MBTS can often be used when MBT is too scorchy. Compounds cased on MBTS have slightly better aging and reversion resistance than corresponding ones based on sulfenamides. It can be boosted by use of secondary accelerators to achieve a faster cure and higher modulus.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/cc
Molecular Weight 332.5 g/mol
Ash <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 166 °CInitial
 
Descriptive Properties
AppearanceGray-white powder
Assay content>95%
Content<0.1%Residues (150µm)
 <1%Free MBT
Loss on drying<0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS006 / 316588

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.