MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 7316 PBT, 35% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Celanex 7316 is a non-exuding (UL and CSA approved V-0 at 1/32 inch), 35% glass/mineral reinforced PBT, which has an excellent balance of mechanical properties and processability. It is well suited for electrical applications where warp resistance is req
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours.
For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.

Information provided by Celanese Corporation.

Key Words: 35% glass/mineral, V-0, non-exuding, higher CTI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/ccASTM D792
Density 1.74 g/ccISO 1183
Water Absorption 0.10 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 43ISO 2039-2
Tensile Strength at Break 80.0 MPa5mm/min; ISO 527-2/1A
 11000 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 1.8 %5mm/min; ISO 527-2/1A
 1.9 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 9200 MPa1mm/min; ISO 527-2/1A
Flexural Strength 130 MPaISO 178
 17500 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 9450 MPaISO 178
 1.40e+6 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²ISO 180/1A
Charpy Impact Unnotched 29.0 kJ/m²ISO 179/1eU
 29.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.70 kJ/m²ISO 179/1eA
 6.70 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 470 V/milshort term; ASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 123 secASTM D495
Comparative Tracking Index 300 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 55.0 µm/m-°CISO 11359-2
Melting Point 225 °CISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 212 °CISO 75-1, -2
 417 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 184 °CISO 75-1, -2
 383 °FASTM D648
Glass Transition Temp, Tg 60.0 °CISO 11357-1,-2,-3
Flammability, UL94 V-0
 V-0
@Thickness 0.850 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 50.0 °Chopper
 65.0 - 96.0 °Ccavity
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 255 °C
Die Temperature 240 - 255 °C
Melt Temperature 235 - 255 °C
 260 °CISO 294
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4 hour
Moisture Content 0.020 %Necessary low maximum
Injection Pressure 48.0 MPaISO 294
Hot-Working Temperature 250 - 260 °C
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCS095 / 123510

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.