MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Verdant Specialty Solutions MIRANOL® ULTRA L 32 E Surfactant
Categories: Fluid

Material Notes: Description: Functions as a mild emulsifier, solubilizer and foaming agent. Its high foaming property and ability to reduce the irritation of other surfactants finds use in both liquid dish detergents and liquid hand soaps. Due to its wide pH stability it can be used in a variety of acidic or alkaline hard surface cleaners.

C.T.F.A. /I.N.C.I. Name: SODIUM LAUROAMPHOACETATE

CAS: 68608 – 66 – 2

EINECS: 271 – 794 – 6

Available in: Asia Pacific, Europe, Latin America and North America

Stability: Stable with stong acids, neutral, strong alkalis.

Solubility: Water, ethanol

Compatibility: Compatible with electrolyte solutions and with anionic, cationic, non-ionic surfactants.

Ionic character: Amphoteric

Applications: Aqueous solution of an amphoteric surfactant from a Lauric base. Ultra pure mild surfactant, that can reduce the irritancy of other surfactants (like commonly used anionic :SLES, SLS). Recommended for use in baby shampoos, baby bath products. Exceptional foam quality in blends with sulfates surfactants as compared to betaines. Synergie with cationic guars.

Information provided by Rhodia, Rhodia has been acquired by Solvay. Verdant Specialty Solutions was created through the purchase of Solvay's amphoteric and secondary surfactants business

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Solids Content 38 - 39.5 %L250
pH 9.0 - 1020% aq. Sol.; L115
Viscosity <= 10000 cPcalculated: Solids-(NaCl + Sodium Glycolate); L170
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0L039/L038
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear clean liquid
CompositionActive30-32%, L401
 Na Glycolate<1.8%, L403
 Sodium Chloride<7.6%, L400
Foam Volume360 cm3at pH 6, 0.1 active materials, in hard or distilled water, N.F.T. standard 73404
OdorFaint, characteristic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD263 / 137494

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.