MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) RHODAPON® LSB/STD Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODAPON® LSB/STD is a high foaming detergent with excellent emulsification and wetting properties for use in glass, hard-surface cleaners and other institutional applications. RHODAPON® LSB/STD is also useful in hair color treatments, shampoos, bath products and other related cosmetic products

Chemical Name: Sodium 2-Ethylhexyl Sulfate

CAS No: 126-92-1

EINECS No: 204-812-8

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
pH 7.5 - 8.510% Solution; RP-0420
Viscosity <= 250 cPRP-0596
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear LiquidRP-0064
Cloud point<20°CRP-0123
Color<85APHA, 50% Solution, RP-0134
Content<0.3%Sodium Chloride, RP-0098
 <1.5%Sodium Sulfate, RP-0555
 <5 ppmIron as FE, (O-Phenanthroline), RP-0277
 0.9-2%Unsulfated Matter, RP-17303
 27.8-29%Active, Eq Wt 305, RP-0033
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ametek Tungsten-Copper Composites AWC 8812
Ametek Tungsten-Copper Composites AWC 8515
Ametek Tungsten-Copper Composites AWC 8020
Ametek Tungsten-Copper Composites AWC 7525
Borosilicate Glass, Low Expansion

PSOLVAY781 / 218509

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.