MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ho Hsiang Ching HA-700W SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The HA series belongs to the SEBS (STYRENE-ETHYLENE/BUTYLENE- STYRENE) hydrogenated and alloyed grade of materials. The materials of the HA series are slip resistant, soft and comfortable, look good and has excellent mechanical strength and scratch resistance. It can be combined with ABS and PC materials with excellent shot sticky strength. When used in high precision steel mold production, no matter what the finished product is accessory or small part, its products are able to reach an excellent level of consistency and function. For example, the thermoplastic elastomer material (TPE/TPS) in coating on 3C product and medical product is a good choice with regards to both performance and value. HHC's HA series can meet the needs of such commercialization, and it is the best choice for customers' needs! Suitable for most of the thermoplastic processing methods, such as injection molding, extrusion molding and so on. This material complies with EU RoHS, REACH-SVHC regulations and has passed the Nylon Phenol Ethoxylates (NPEO), Polynuclear aromatic hydrocarbons (PAHs) and phthalates (6P, Nylonphenol) and other safety tests. It is a non-toxic and safe material with environmentally friendly specifications.

Color: Natural Color / Black Color / Customized Color

The optimum combination of materials: ABS, PC

Processing: Injection, Extrusion

Storage conditions: At room temperature, avoid direct sunlight, keep away from fire and avoid humid environment.

Applications: Sport goods, pneumatic tools, power tools, etc.

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength 59.0 kg(f)/cm²ASTM 412C
Elongation at Break 575 %ASTM 412C
Tear Strength 27.0 kg(f)/cmASTM 412C
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 100 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 160 - 177 °C
Middle Barrel Temperature 166 - 182 °C
Front Barrel Temperature 177 - 191 °C
Nozzle Temperature 182 - 204 °C
Mold Temperature 16.0 - 66.0 °C
Injection Velocity 13.0 - 25.0 mm/sec
Injection Pressure 34.0 - 69.0 MPa
Hold Pressure 14.0 - 48.0 MPa
Back Pressure 0.340 - 0.690 MPa
Screw Speed 50 - 70 rpm
 
Descriptive Properties
Cold resistance temperature-50°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHSIANG049 / 312525

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.